CompareMaterialsMaterial DescriptionCertificatesReference PriceOperate
PP Copolymer 4Plas 5C40800
melt mass-flow rate 35 Impact strength of cantilever beam gap 3.0 tensile strength 25.0
-- --
POM 4Plas 23I10000
tensile strength 67.0 Bending modulus 2700 melt mass-flow rate 9.0
-- --
PP Copolymer 4Plas 9C12420 IUV
melt mass-flow rate 5.0 Impact strength of cantilever beam gap 10 tensile strength 7.00 Filler glass fiber reinforced material 20% filler by weight
-- --
ABS 4Plas 10H20000 A-M
Impact strength of cantilever beam gap 15 melt mass-flow rate 12to16 Hot deformation temperature 97.0 tensile strength 43.0
-- --
PP 4Plas 9C11270
melt mass-flow rate 5.0 Impact strength of cantilever beam gap 12 tensile strength 18.0 Filler barium sulfate
-- --
TPU 4Plas 9T22130 H
Shore hardness 65.0 Tensile strain 15 tensile strength 70.0 Filler glass fiber reinforced material 30% filler by weight
-- --
PA6 4Plas 9B22135
Water absorption rate 1.9 tensile strength 185 Hot deformation temperature 220 Filler glass fiber reinforced material 35% filler by weight
-- --
PA66 4Plas 9A23300 X
Water absorption rate 2.7 tensile strength 85.0 Hot deformation temperature 210
-- --
PP Copolymer 4Plas 9C19300
melt mass-flow rate 9.0 Impact strength of cantilever beam gap 25 Hot deformation temperature 45.0 tensile strength 20.0
-- --
PP 4Plas 25C21120
melt mass-flow rate 15 Impact strength of cantilever beam gap 4.0 Bending modulus 2.30 tensile strength 23.0 Filler reinforcement material talc filler 20% filler by weight characteristics copolymer
-- --
PA66 4Plas 9A22115 I
Water absorption rate 1.5 tensile strength 130.0 Hot deformation temperature 240 Filler reinforcement material glass fiber reinforcement material 15% filler additive by weight impact modifier characteristics impact modification
-- --
PA6 4Plas 9B22145 HUVW
Water absorption rate 1.6 tensile strength 210 Hot deformation temperature 220 Filler glass fiber reinforced material 45% filler by weight
-- --
PA6 4Plas 9B22330 H
Water absorption rate 2.1 tensile strength 110 Hot deformation temperature 210 Filler glass bead glass fiber 30% filler by weight
-- --
PA6 4Plas 9B22115 XHFR1
Water absorption rate 1.7 tensile strength 100 Filler glass fiber reinforced material 15% filler by weight
-- --
PA66 4Plas 9AB22120 HUV2
Water absorption rate 1.2 tensile strength 125 Hot deformation temperature 230 Filler glass fiber reinforced material 20% filler by weight
-- --
PC+PBT 4Plas 9KF23500 HI
melt mass-flow rate 60 Impact strength of cantilever beam gap 8.0 Hot deformation temperature 130 tensile strength 45.0
-- --
PC 4Plas 10F23100 X
Impact strength of cantilever beam gap 10 Hot deformation temperature 136 tensile strength 60.0
-- --
PBT+PET 4Plas 9KL32130
melt mass-flow rate 40 Impact strength of cantilever beam gap 7.0 Hot deformation temperature 195 tensile strength 130 Filler glass fiber reinforced material 30% filler by weight
-- --
PA6 4Plas 9B22115 HFR1
Water absorption rate 1.7 tensile strength 100 Hot deformation temperature 195 Filler glass fiber reinforced material 15% filler by weight
-- --
ABS 4Plas 10E17300
Impact strength of cantilever beam gap 42 Hot deformation temperature 125 tensile strength 55.0
-- --