PA66 9A22115 I 4Plas
Properties:
Filler reinforcement material glass fiber reinforcement material 15% filler additive by weight impact modifier characteristics impact modification
Product Description
Certificates(0)
Datasheet
Product Description
| Properties: | Filler | reinforcement material | glass fiber reinforcement material | 15% | filler additive by weight | impact modifier characteristics | impact modification |
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8 | kJ/m² |
| Tensile modulus | 23°C | ISO 527-2 | 6300 | MPa |
| Elongation at Break | 23°C | ISO 527-2 | 5 | % |
| tensile strength | 23°C | ISO 527-2 | 130 | MPa |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 8.0 | kJ/m² |
| -30°C | ISO 180/1A | 7.0 | kJ/m² | |
| Tensile strain | Break, 23°C | ISO 527-2/5 | 5.0 | % |
| tensile strength | Break, 23°C | ISO 527-2/5 | 130.0 | MPa |
| Tensile modulus | 23°C | ISO 527-2/5 | 6300 | MPa |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Melting temperature | ISO 11357-3 | 263 | °C | |
| Vicat softening temperature | ISO 306/B50 | 255 | °C | |
| Hot deformation temperature | 1.80MPaUnannealed | ISO 75-2/Af | 225 | °C |
| 0.45MPaUnannealed | ISO 75-2/Bf | 240 | °C | |
| Melting temperature | ISO 11357 | 263 | °C | |
| Vicat softening temperature | ISO 306/B | 255 | °C | |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 225 | °C |
| 0.45 MPa, Unannealed | ISO 75-2/B | 240 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 1.5 | % |
| Shrinkage rate | TD | ISO 2557 | 1.2 | % |
| density | ISO 1183 | 1.24 | g/cm³ | |
| Shrinkage rate | TD | ISO 294-4 | 1.2 | % |
| MD | ISO 294-4 | 0.4 | % | |
| density | ISO 1183 | 1.24 | g/cm³ | |
| Water absorption rate | 23°C,50RH | ISO 62 | 1.5 | % |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Compared to the anti leakage trace index | IEC 60112 | PLC 1 | ||
| other | 灼热丝易燃指数,2.00 mm | IEC 60695-2-12 | 650 | °C |
| UL 阻燃等级,1.60 mm | UL 94 | HB | ||
| Compared to the anti leakage trace index | IEC 60112 | PLC 1 | ||
| flame retardancy | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | Allcolor | UL -94 | HB | 1.60mm |
| Relative temperature of heating wire | 2.00mm | IEC 60695-2-12 | 650 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.