Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
密度 | ASTMD792 | 0.955 g/cm³ | |
熔体质量流动速率 | 190°C/2.16kg | ASTMD1238 | 0.35 g/10min |
190°C/21.6kg | ASTMD1238 | 30 g/10min |
薄膜 | Test Condition | Test Method | Test Result |
---|---|---|---|
薄膜厚度-经测试 | 25 µm | ||
割线模量 | 25µm,BlownFilm | ASTMD882A | 917 MPa |
25µm,BlownFilm | ASTMD882A | 1280 MPa | |
拉伸强度 | Yield,25µm,BlownFilm | ASTMD882A | 27.6 MPa |
Yield,25µm,BlownFilm | ASTMD882A | 29.6 MPa | |
拉伸应变-MD | Break,25µm,BlownFilm | ASTMD882A | 500 % |
拉伸应变 | Break,25µm,BlownFilm | ASTMD882A | 25 % |
落锤冲击 | 25µm,吹塑薄膜 | ASTMD1709A | <50 g |
ElmendorfTearStrength-MD | 25µm,BlownFilm | ASTMD1922 | 8.0 g |
ElmendorfTearStrength-TD | 25µm,BlownFilm | ASTMD1922 | 1100 g |
WaterVaporTransmissionRate | 38°C,25µm,BlownFilm | ASTMF1249 | 11 g/m²/24hr |
拉伸强度 | Break,25µm,BlownFilm | ASTMD882A | 43.4 MPa |
Break,25µm,BlownFilm | ASTMD882A | 29.6 MPa |
热性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
熔融峰值温度 | ASTMD3417 | 132 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.