Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO 62 | 2.5 % |
density | | ISO 1183 | 5.20 g/cm³ |
Water absorption rate | | ISO 62 | 0.80 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of simply supported beam without notch | | ISO 179/1eU | 26 kJ/m² |
Charpy Notched Impact Strength | | ISO 179/1eA | 3.0 kJ/m² |
Charpy Notched Impact Strength | | ISO 179/1eA | 4.0 kJ/m² |
Impact strength of simply supported beam without notch | | ISO 179/1eU | 20 kJ/m² |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO 527-2 | 1500 MPa |
tensile strength | | ISO 527-2 | 18.0 MPa |
Tensile strain | | ISO 527-2 | 22 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Volume resistivity | | IEC 60093 | 1E+09 ohms·cm |
Surface Resistivity | | IEC 60093 | 1E+08 ohms |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Heat distortion temperature | | ISO 75-2/B | 225 °C |
Heat distortion temperature | | ISO 75-2/A | 220 °C |
Continuous use temperature | | IEC 60216 | 100 °C |
ball-indentation hardness | | IEC 60695-10-2 | 通过 |
ball-indentation hardness | | IEC 60695-10-2 | 通过 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.