POM FW-24 HANYANG KOREA
0
- Properties:Wear resistant oil containing system
Technical Data Sheet
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | ASTM D-1238 | 9 g/10min |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | 23℃ | ASTM D-638 | 520 kgf/cm |
| Impact strength of cantilever beam gap | Notch t3.2mm | ASTM D-256 | 5.0 kgf.cm/cm |
| Bending modulus | 23℃ | ASTM D-790 | 2.50 ×10 |
| elongation | 23℃ | ASTM D-638 | 50 % |
| Impact strength of cantilever beam gap | t3.2mm S type | ASTM D-1822 | 80 kgf.cm/cm |
| bending strength | 23℃ | ASTM D-790 | 750 kgf/cm |
| Rockwell hardness | M scale | ASTM D-785 | M80 |
| Elongation at Break | t2mm | ASTM D-732 | 520 kgf/cm |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melting temperature | 10C°/min | DSC Method | 165 ℃ |
| Hot deformation temperature | 18.6kgf/cm | ASTM D-648 | 107 ℃ |
| 4.6kgf/cm | ASTM D-648 | 156 ℃ | |
| Combustibility | t0.8mm | UL 94 | HB |
| Linear coefficient of thermal expansion | 20℃-80℃ | ASTM D-696 | 13 ×10 |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D-792 | 1.41 | |
| filler content | 高 % | ||
| Water absorption rate | 23°C,60%RH | ASTM D-570 | 0.22 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Volume resistivity | ASTM D-257 | 1×10 欧姆.cm | |
| Shrinkage rate | t3mm,直径100mm | ASTM D-149 | 2.0 % |
| Surface resistivity | ASTM D-257 | 1×10 欧姆 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.