Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM FW-24 HANYANG KOREA
--
--
Wear resistance, oil bearing system
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic performance | Test Condition | Test Method | HANYANG KOREA/FW-24 |
---|---|---|---|
melt mass-flow rate | ASTM D-1238 | 9 g/10min |
Electrical performance | Test Condition | Test Method | HANYANG KOREA/FW-24 |
---|---|---|---|
Surface Resistivity | ASTM D-257 | 1×10 欧姆 | |
Volume resistivity | ASTM D-257 | 1×10 欧姆.cm | |
Shrinkage rate | t3mm,直径100mm | ASTM D-149 | 2.0 % |
Mechanical properties | Test Condition | Test Method | HANYANG KOREA/FW-24 |
---|---|---|---|
Impact strength of cantilever beam gap | t3.2mm S type | ASTM D-1822 | 80 kgf.cm/cm |
elongation at break | t2mm | ASTM D-732 | 520 kgf/cm |
bending strength | 23℃ | ASTM D-790 | 750 kgf/cm |
Flexural modulus | 23℃ | ASTM D-790 | 2.50 ×10 |
Impact strength of cantilever beam gap | Notch t3.2mm | ASTM D-256 | 5.0 kgf.cm/cm |
tensile strength | 23℃ | ASTM D-638 | 520 kgf/cm |
Rockwell hardness | M scale | ASTM D-785 | M80 |
elongation | 23℃ | ASTM D-638 | 50 % |
physical property | Test Condition | Test Method | HANYANG KOREA/FW-24 |
---|---|---|---|
filler content | 高 % | ||
Water absorption rate | 23°C,60%RH | ASTM D-570 | 0.22 % |
density | ASTM D-792 | 1.41 |
Thermal performance | Test Condition | Test Method | HANYANG KOREA/FW-24 |
---|---|---|---|
Heat distortion temperature | 4.6kgf/cm,HDT | ASTM D-648 | 156 ℃ |
combustibility | t0.8mm | UL 94 | HB |
Heat distortion temperature | 18.6kgf/cm,HDT | ASTM D-648 | 107 ℃ |
melting temperature | 10C°/min | DSC Method | 165 ℃ |
Linear coefficient of thermal expansion | 20℃-80℃ | ASTM D-696 | 13 ×10 |