PP Copolymer Jampilen H2464

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11830.900 g/cm³
melt mass-flow rateISO 11330.30 g/10min
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-2/11350 MPa
tensile strength YieldISO 527-2/5029.0 MPa
Tensile strainYieldISO 527-2/5010 %
Tensile strainBreakISO 527-2/50400 %
Flexural modulusISO 1781450 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO 1809.0 kJ/m²
Impact strength of cantilever beam gapISO 18017 kJ/m²
Impact strength of cantilever beam gapISO 18035 kJ/m²
Impact strength of cantilever beam gapISO 18066 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
Oxygen induction timeEN728>30 min
Oxygen induction timeEN728>15 min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.