Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Copolymer Jampilen H2464 Jam Polypropylene Company
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2464 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ISO 180 | 66 kJ/m² |
-20°C | ISO 180 | 17 kJ/m² | |
-30°C | ISO 180 | 9.0 kJ/m² | |
0°C | ISO 180 | 35 kJ/m² |
Mechanical properties | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2464 |
---|---|---|---|
Flexural modulus | ISO 178 | 1450 MPa | |
Tensile strain | 断裂 | ISO 527-2/50 | 400 % |
Tensile modulus | ISO 527-2/1 | 1350 MPa | |
Tensile strain | 屈服 | ISO 527-2/50 | 10 % |
tensile strength | 屈服 | ISO 527-2/50 | 29.0 MPa |
physical property | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2464 |
---|---|---|---|
density | ISO 1183 | 0.900 g/cm³ | |
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 0.30 g/10min |
Thermal performance | Test Condition | Test Method | Jam Polypropylene Company/Jampilen H2464 |
---|---|---|---|
Oxygen induction time | 200°C | EN728 | >30 min |
210°C | EN728 | >15 min |