Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.15到1.17 g/cm³ |
Water absorption rate | | ASTMD570 | 1.2 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | | ASTMD785 | 115 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
bending strength | | ASTMD790 | 86.2 MPa |
Tensile modulus | | ASTMD638 | 2410 MPa |
tensile strength | | ASTMD638 | 75.8 MPa |
elongation | | ASTMD638 | 20 % |
Flexural modulus | | ASTMD790 | 2410 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Suspended wall beam without notch impact strength | | ASTMD256 | 32 J/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | ASTMD149 | 20 kV/mm |
dielectric constant | | ASTMD150 | 3.70 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 188 °C |
| | ASTMD648 | 93.3 °C |
melting temperature | | ASTMD2133 | 220 °C |
| | ASTMD696 | 7.2E-05 cm/cm/°C |
maximum service temperature | | | 149 °C |
maximum service temperature | | UL746B | 93 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.