Technical Data Sheet
Cured Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTMD638 | 1.03 MPa | |
elongation | Break | ASTMD638 | 450 % |
tear strength | ASTMD624 | 4.38 kN/m | |
Supporting hardness | ASTMD2240 | 5到15 |
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | Base Resin | 1.05 g/cm³ | |
1.06 g/cm³ | |||
1.07 g/cm³ | |||
Shrinkage rate | ASTMD2566 | 0.10到0.30 % |
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Resin | 按重量计算的混合比:100按容量计算的混合比:100 | ||
Hardener | 按重量计算的混合比:100按容量计算的混合比:98 | ||
Demold Time | 180到300 min |
Uncured Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
0.20 Pa·s | |||
0.60 Pa·s | |||
1.5 Pa·s | |||
1.7E+02 hr | |||
10到14 min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.