PA6 GLS Nylon 6 PG39

0
  • Properties:
    Filler
    glass fiber reinforced material
    15%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.20to1.24 g/cm³
Shrinkage rateASTM D9550.30to0.60 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength YieldASTM D638>100 MPa
elongationBreakASTM D6382.0to6.0 %
Flexural modulusASTM D790>4000 MPa
bending strengthASTM D790>130 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D256>40 J/m
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648>150 °C
Heat distortion temperatureASTM D648>58.0 °C
vicatASTM D15254>210 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.