Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 GLS Nylon 6 PG39 GLS Polymers Pvt. Ltd.
--
--
Filler, glass fiber reinforced material, 15%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | GLS Polymers Pvt. Ltd./GLS Nylon 6 PG39 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | >58.0 °C |
| 0.45MPa,Unannealed | ASTM D648 | >150 °C | |
| Vicat softening temperature | ASTM D15254 | >210 °C |
| mechanical properties | Test Condition | Test Method | GLS Polymers Pvt. Ltd./GLS Nylon 6 PG39 |
|---|---|---|---|
| Bending modulus | ASTM D790 | >4000 MPa | |
| bending strength | ASTM D790 | >130 MPa | |
| elongation | Break | ASTM D638 | 2.0to6.0 % |
| tensile strength | Yield | ASTM D638 | >100 MPa |
| Physical properties | Test Condition | Test Method | GLS Polymers Pvt. Ltd./GLS Nylon 6 PG39 |
|---|---|---|---|
| density | ASTM D792 | 1.20to1.24 g/cm³ | |
| Shrinkage rate | MD:3.20mm | ASTM D955 | 0.30to0.60 % |
| impact performance | Test Condition | Test Method | GLS Polymers Pvt. Ltd./GLS Nylon 6 PG39 |
|---|---|---|---|
| Impact strength of cantilever beam gap | 3.20mm | ASTM D256 | >40 J/m |
| flammability | Test Condition | Test Method | GLS Polymers Pvt. Ltd./GLS Nylon 6 PG39 |
|---|---|---|---|
| UL flame retardant rating | 3.0mm | UL 94 | HB |