PA66 528BR-WO USA Axiall

0
  • Properties:
    Drying temperature
    65
    6-71
    1 ℃
    drying time
    2-3 hours
    screw barrel rear temperature
    282 ℃
    middle temperature
    274 ℃
    front temperature
    271 ℃
    nozzle temperature
    260-299 ℃
    mold temperature
    37
    8-93
    3 ℃

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.25 g/cm3
Mechanical propertiesTest ConditionTest MethodTest Result
Rockwell hardnessASTM D785119
Test ConditionTest MethodTest Result
Heat distortion temperatureASTM D64862.8
melting temperatureASTM D648254
UL flame retardant ratingV-0
bending strengthASTM D790101 MPa
Impact strength of cantilever beam gapASTM D25648.0 J/m
tensile strength ASTM D63867.6 MPa
dielectric strengthASTM D14922 kV/mm
dielectric constantASTM D1503.7
Shrinkage rateASTM D9551.5 %
Water absorption rateASTM D5701.1 %
Water absorption rateASTM D570--- %
elongationASTM D63820 %
Flexural modulusASTM D7902900 MPa
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTM D2571E+16 ohm.cm
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648207
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.