PA66 528BR-WO USA Axiall
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Test Condition | Test Method | USA Axiall/528BR-WO | |
---|---|---|---|
tensile strength | ASTM D638 | 67.6 MPa | |
Water absorption rate | 饱和 | ASTM D570 | --- % |
elongation | 断裂 | ASTM D638 | 20 % |
Shrinkage rate | 流动 | ASTM D955 | 1.5 % |
dielectric strength | ASTM D149 | 22 kV/mm | |
Impact strength of cantilever beam gap | ASTM D256 | 48.0 J/m | |
Water absorption rate | 24小时 | ASTM D570 | 1.1 % |
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 62.8 ℃ |
melting temperature | ASTM D648 | 254 ℃ | |
dielectric constant | 1MHz | ASTM D150 | 3.7 |
Flexural modulus | ASTM D790 | 2900 MPa | |
UL flame retardant rating | UL 94 | V-0 | |
bending strength | ASTM D790 | 101 MPa |
Mechanical properties | Test Condition | Test Method | USA Axiall/528BR-WO |
---|---|---|---|
Rockwell hardness | R计称 | ASTM D785 | 119 |
Electrical performance | Test Condition | Test Method | USA Axiall/528BR-WO |
---|---|---|---|
Volume resistivity | ASTM D257 | 1E+16 ohm.cm |
physical property | Test Condition | Test Method | USA Axiall/528BR-WO |
---|---|---|---|
density | ASTM D792 | 1.25 g/cm3 |
Thermal performance | Test Condition | Test Method | USA Axiall/528BR-WO |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTM D648 | 207 ℃ |