UHMWPE GUR®  X 188 CELANESE USA

12

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Charpy Notched Impact Strength23°CISO 11542-290.0 kJ/m²
mechanical propertiesTest ConditionTest MethodTest Result
Wear by Sandslurry MethodInternal Method200
Nominal tensile fracture strainISO 527-2/1B800 %
Tensile strainYieldISO 527-2/1B8.0 %
tensile strength50% StrainISO 527-2/1B18.0 Mpa
tensile strengthBreakISO 527-2/1B38.0 Mpa
tensile strengthYieldISO 527-2/1B24.0 Mpa
Tensile modulusISO 527-2/1B950 Mpa
thermal performanceTest ConditionTest MethodTest Result
Vicat softening temperatureISO 306/B5080.0 °C
Physical propertiesTest ConditionTest MethodTest Result
Apparent densityISO 600.45 g/cm³
melt mass-flow rate190°C/21.6 kgISO 11330.50 g/10 min
Particle size distributiond115
average molecular weight700000 g/mol
StickinessElongational Stress F - 150/10ISO 11542-2< 0.0500 Mpa
Stickiness--2ISO 1628600.0 ml/g
Stickiness--ISO 1628600.0 ml/g
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.