Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|---|---|---|
密度 | ASTMD792 | 1.16 g/cm³ | |
ISO1183 | 1.16 g/cm³ | ||
ApparentViscosity | 190°C,300sec^-1 | ASTMD3835 | 630 Pa·s |
弹性体 | Test Condition | Test Method | Test Result |
---|---|---|---|
伸长率 | Break | ISO37 | 550 % |
TearStrength | 24°C | ASTMD624 | 40.3 kN/m |
24°C | ISO34-1 | 40 kN/m | |
压缩永久变形 | 24°C,22hr | ASTMD395A | 21 % |
100°C,22hr | ASTMD395A | 70 % | |
24°C,22hr | ISO815 | 21 % | |
100°C,22hr | ISO815 | 70 % | |
拉伸永久变形 | ASTMD412 | 13 % | |
拉伸应力 | 100%应变 | ASTMD412 | 4.69 MPa |
100%应变 | ISO37 | 4.69 MPa | |
抗张强度 | Yield | ASTMD412 | 11.0 MPa |
拉伸应力 | Yield | ISO37 | 11.0 MPa |
伸长率 | Break | ASTMD412 | 550 % |
老化 | Test Condition | Test Method | Test Result |
---|---|---|---|
体积变化 | 100°C,168hr,inIRM903Oil#3 | ASTMD471 | 29 % |
100°C,168hr,在水中 | ASTMD471 | -10 % | |
100°C,168hr,inASTM#1Oil | ISO1817 | 17 % | |
100°C,168hr,在水中 | ISO1817 | -10 % | |
空气中拉伸强度的变化率 | 125°C,168hr | ASTMD573 | 96 % |
100%Strain,125°C,168hr | ASTMD573 | 83 % | |
125°C,168hr | ISO188 | 96 % | |
100%应变125°C,168hr | ISO188 | 83 % | |
体积变化 | 100°C,168hr,inASTM#1Oil | ASTMD471 | 17 % |
100°C,57120hr,inIRM903Oil#3 | ISO1817 | 29 % |
硬度 | Test Condition | Test Method | Test Result |
---|---|---|---|
肖氏硬度 | Shore A | ASTMD2240 | 79 |
Shore A | ISO868 | 79 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App