| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | 100%Strain | ASTM D412 | 15.0 MPa |
| 300%Strain | ASTM D412 | 18.0 MPa | |
| ASTM D412 | 30.0 MPa | ||
| elongation | Break | ASTM D412 | 380 % |
| tear strength | ASTM D624 | 0.150 kN/m | |
| Permanent compression deformation | 23°C,70hr | ASTM D395B | 26 % |
| 70°C,24hr | ASTM D395B | 32 % |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Wear amount | DIN 53516 | 40.0 mm³ |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Glass transition temperature | ASTM D3418 | -12.0 °C | |
| Melting temperature | 185to200 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D792 | 1.12 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 88to92 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.