TPU-Ether Utomer UT590 Shanghai Utomer Material Science Co., Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT590 |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 88to92 |
| thermal performance | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT590 |
|---|---|---|---|
| Glass transition temperature | ASTM D3418 | -12.0 °C | |
| Melting temperature | 185to200 °C |
| mechanical properties | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT590 |
|---|---|---|---|
| Wear amount | DIN 53516 | 40.0 mm³ |
| Physical properties | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT590 |
|---|---|---|---|
| density | ASTM D792 | 1.12 g/cm³ |
| elastomer | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT590 |
|---|---|---|---|
| elongation | Break | ASTM D412 | 380 % |
| Permanent compression deformation | 70°C,24hr | ASTM D395B | 32 % |
| 23°C,70hr | ASTM D395B | 26 % | |
| tear strength | ASTM D624 | 0.150 kN/m | |
| tensile strength | ASTM D412 | 30.0 MPa | |
| 300%Strain | ASTM D412 | 18.0 MPa | |
| 100%Strain | ASTM D412 | 15.0 MPa |