PA66 Nypol® PA A3 G35 HS UV RH PRTA010 NR346 Brazil Petropol

0
  • Properties:
    Filler
    glass fiber reinforced material
    35%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.41 g/cm³
Shrinkage rateASTM D9550.20to0.45 %
Water absorption rateEquilibriumASTM D5705.0 %
ash contentASTM D258433to37 %
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessASTM D785120
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ASTM D638175 MPa
elongationBreakASTM D6382.8 %
Flexural modulusASTM D79010300 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D256110 J/m
Electrical performanceTest ConditionTest MethodTest Result
Volume resistivityASTM D2571E+15 ohms·cm
Surface ResistivityASTM D2571E+13 ohms
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648250 °C
melting temperatureASTM D2117261 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.

Contact Us

Get App

Top