PA66 Nypol® PA A3 G35 HS UV RH PRTA010 NR346 Brazil Petropol
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 110 J/m |
hardness | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
Rockwell hardness | R级,23°C | ASTM D785 | 120 |
Electrical performance | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
Volume resistivity | ASTM D257 | 1E+15 ohms·cm | |
Surface Resistivity | ASTM D257 | 1E+13 ohms |
Mechanical properties | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 2.8 % |
tensile strength | ASTM D638 | 175 MPa | |
Flexural modulus | ASTM D790 | 10300 MPa |
flammability | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
physical property | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.20to0.45 % |
ash content | ASTM D2584 | 33to37 % | |
Water absorption rate | 平衡 | ASTM D570 | 5.0 % |
density | ASTM D792 | 1.41 g/cm³ |
Thermal performance | Test Condition | Test Method | Brazil Petropol/Nypol® PA A3 G35 HS UV RH PRTA010 NR346 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 250 °C |
melting temperature | ASTM D2117 | 261 °C |