Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
密度 | | ASTMD792 | 1.17 g/cm³ |
密度 | | ISO1183 | 1.17 g/cm³ |
机械性能 | Test Condition | Test Method | Test Result |
---|
拉伸模量 | 1.91mm,CompressionMolded | ASTMD638 | 2.62 MPa |
拉伸模量 | 1.91mm,CompressionMolded | ISO527-2 | 2.62 MPa |
拉伸强度 | Yield,1.91mm,CompressionMolded | ASTMD638 | 8.45 MPa |
拉伸强度 | Yield,1.91mm,CompressionMolded | ISO527-2 | 8.45 MPa |
拉伸应变 | Break,1.91mm,CompressionMolded | ASTMD638 | 440 % |
TensileStrain | Break,1.91mm,CompressionMolded | ISO527-2 | 440 % |
泰伯耐磨性 | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 4.00 mg |
弹性体 | Test Condition | Test Method | Test Result |
---|
压缩永久变形 | 100°C,22hr | ISO815 | 72 % |
Clash-BergModulus | -40°C | ASTMD1043 | 68.9 MPa |
拉伸永久变形 | | ASTMD412 | 7 % |
TearStrength | 24°C | ASTMD624 | 29.8 kN/m |
压缩永久变形 | 24°C,22hr | ASTMD395B | 16 % |
压缩永久变形 | 100°C,22hr | ASTMD395B | 72 % |
压缩永久变形 | 24°C,22hr | ISO815 | 16 % |
老化 | Test Condition | Test Method | Test Result |
---|
ChangeinShoreHardnessinAir | 125°C,168hr | ISO188 | 54 |
ChangeinUltimateElongation | 125°C,168hr | ASTMD471 | 400 % |
ChangeinDurometerHardness | 125°C,168hr | ASTMD471 | 54 |
体积变化 | 24°C,168hr,inReferenceFuelB | ASTMD471 | 13 % |
体积变化 | 100°C,168hr,inASTM#1Oil | ASTMD471 | -19 % |
体积变化 | 100°C,168hr,inASTM#3Oil | ASTMD471 | 14 % |
体积变化 | 100°C,168hr,在水中 | ASTMD471 | 9.0 % |
硬度 | Test Condition | Test Method | Test Result |
---|
DurometerHardness | ShoreA,1.91mm,CompressionMolded | ASTMD2240 | 57 |
IRHD硬度 | | ISO48 | 57 |
热性能 | Test Condition | Test Method | Test Result |
---|
脆化温度 | | ASTMD746 | -68.9 °C |
脆化温度 | | ISO974 | -68.9 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.