Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD1238 | 0.80 g/10min | ||
melt mass-flow rate | ASTM D-1238 | 0.80 g/10min | |
film thickness | DSC |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTMD1003 | 9.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strength of film | ASTMD882 | 13 Mpa | |
Tensile fracture strength of film | ASTMD882 | 29 Mpa | |
ASTMD882 | 22 Mpa | ||
The elongation at break of the membrane | ASTMD882 | 400 % | |
ASTMD882 | 610 % | ||
ASTM D-1894 | 0.45 | ||
Falling hammer impact | ASTM D-1709 | 74 g | |
tensile yield strength | 13 | ||
tensile breaking strength | ASTM D-882A | 29 MPa | |
22 | |||
1% secant modulus | ASTM D-882 | 230 MPa | |
270 | |||
elongation at break | ASTM D-882 | 400 % | |
610 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | ASTM1525 | 99.8 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.