AES+PC KumhoSunny PC/AES HEC0255B
0
- Properties:Mechanical properties
- Usages:Blow molding applicationsautomotive applications
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | IEC 60093 | >1.0E+15 ohms | |
Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm |
Test Condition | Test Method | Test Result | |
---|---|---|---|
bending strength | ASTM D790 | 75.0 MPa | |
Impact strength of cantilever beam gap | ASTM D256 | 600 J/m | |
Heat distortion temperature | ASTM D648 | 106 °C | |
melt mass-flow rate | ASTM D1238 | 12 g/10min | |
Shrinkage rate | ASTM D955 | 0.40to0.60 % | |
tensile strength | ASTM D638 | 55.0 MPa | |
elongation | Break | ASTM D638 | 80 % |
Flexural modulus | ASTM D790 | 2100 MPa | |
density | ASTM D792 | 1.11 g/cm³ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.