Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
PolystyreneContent | 内部方法 | 14到17 % | |
molecular weight | 内部方法 | 207000到237000 g/mol | |
Ash Content | ISO247 | 0.10到0.40 % | |
ISO247 | 2.5到5.0 % | ||
ISO247 | 0.10到0.40 % | ||
ISO247 | <0.20 % | ||
Volatile compounds | 内部方法 | <0.30 % | |
density | ISO2781 | 0.920 g/cm³ | |
Apparent density | ASTMD1895B | 0.35 g/cm³ | |
melt mass-flow rate | ISO1133 | 9.0 g/10min | |
Solution viscosity | 内部方法 | 1200 mPa·s | |
AntioxidantAdditive | 内部方法 | >0.060 % | |
Extractable | 内部方法 | <1.0 % |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO868 | 30 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
CouplingEfficiency | 内部方法 | 78到84 % |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
elongation | Break | ISO37 | 1300 % |
Tensile stress | ISO37 | 0.900 MPa | |
Yield | ISO37 | 28.0 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.