plas
Log In

IR SIBUR Synthetic Rubber IR SKI-3 NST Group II SIBUR RUSSIA

0

Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
elongationBreakASTM D3403>500 %
tensile strengthYieldASTM D3403>27.0 MPa
tensile strength300%StrainASTM D3403>7.00 MPa
Physical propertiesTest ConditionTest MethodTest Result
Volatile compoundsASTM D5668<1.5 %
ash contentASTM D5667<0.50 %
Stearic AcidInternal Method0.50to1.5 %
Mooney viscosityML1+4,100°CASTM D164665to75 MU
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.