Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

IR SIBUR Synthetic Rubber IR SKI-3 NST Group II SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
elastomer | Test Condition | Test Method | SIBUR RUSSIA/SIBUR Synthetic Rubber IR SKI-3 NST Group II |
---|---|---|---|
tensile strength | 屈服 | ASTM D3403 | >27.0 MPa |
300%应变 | ASTM D3403 | >7.00 MPa | |
elongation | 断裂 | ASTM D3403 | >500 % |
physical property | Test Condition | Test Method | SIBUR RUSSIA/SIBUR Synthetic Rubber IR SKI-3 NST Group II |
---|---|---|---|
Stearic Acid | 内部方法 | 0.50to1.5 % | |
Volatile compounds | ASTM D5668 | <1.5 % | |
Mooney viscosity | ML1+4,100°C | ASTM D1646 | 65to75 MU |
ash content | ASTM D5667 | <0.50 % |