physical property Test ConditionTest MethodTest Result
densityASTMD792A,ISO11831.75 g/cm³
Water absorption rateASTMD5700.35 %
Water absorption rateISO620.35 %
Mechanical propertiesTest ConditionTest MethodTest Result
Flexural modulusASTMD79015200 MPa
Flexural modulusISO17815000 MPa
bending strengthASTMD790,ISO178138 MPa
compressive strengthASTMD695,ISO604169 MPa
tensile strengthYieldASTMD63867.6 MPa
tensile strengthYieldISO527-268.0 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256A120 J/m
Impact strength of cantilever beam gapISO180/2A12 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
dielectric strengthASTMD149130 kV/mm
dielectric strengthIEC60243-111 kV/mm
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648,ISO75-2/A360 °C
ISO11359-23.7E-05 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.