Technical Data Sheet
AcidGasEmission-HBr | Test Condition | Test Method | Test Result |
---|---|---|---|
AcidGasEmission-HBr | CSAC22.2No.0.3Method2 | 3.7 % |
Test Condition | Test Method | Test Result | |
---|---|---|---|
brittle temperature | ASTMD746 | <-75.0 °C | |
deformation | UL1581 | 1.0 % | |
HotElongation | 内部方法 | 40 % | |
insulation resistance | UL1581 | 50000 Mohms/1000ft | |
Limiting Oxygen Index | ASTMD2863 | 24 % | |
CrushingTest | UL1581 | 635029 g | |
density | ASTMD792 | 1.01 g/cm³ | |
melt mass-flow rate | ASTMD1238 | 0.80 g/10min | |
The degree of cross combination | ASTMD2765 | 67 % | |
tensile strength | Yield | UL1581 | 12.4 MPa |
Break | UL1581 | 13.8 MPa | |
UL1581 | 13.4 MPa | ||
UL1581 | 12.8 MPa | ||
UL1581 | 12.6 MPa | ||
elongation | Break | UL1581 | 380 % |
UL1581 | 350 % | ||
dielectric constant | ASTMD150 | 2.34 | |
ASTMD150 | 2.34 | ||
UL1581 | 2.50 | ||
Dissipation Factor | ASTMD150 | 1.2E-03 | |
ASTMD150 | 8E-04 | ||
DielectricBreakdown | UL1581 | 35000 V | |
UL1581 | 33000 V | ||
insulation resistance | UL1581 | 560000 Mohms/1000ft | |
UL1581 | 21000 Mohms/1000ft | ||
elongation | UL1581 | 330 % | |
WeatherometerAging | UL1581 | 430 % | |
UL1581 | 440 % | ||
UL1581 | 18.3 MPa | ||
UL1581 | 19.8 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.