PUR-Ester Vibrathane® 6012 CHEMTURU USA
0
Technical Data Sheet
| Uncured Properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Curing time | 110°C | 1.0 hr |
| elastomer | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | 100%Strain | ASTM D412 | 10.3 MPa |
| ASTM D412 | 53.8 MPa | ||
| elongation | Break | ASTM D412 | 430 % |
| tear strength | --2 | ASTM D624 | 133 kN/m |
| Split | ASTM D470 | 25 kN/m | |
| Shore hardness | ASTM D2632 | 24 % | |
| Permanent compression deformation | 70°C,22hr | ASTM D395B | 52 % |
| thermosetting | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Post curing time | 110°C | 4.0 hr |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Brittle temperature | ASTM D746 | -58.0 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| density | ASTM D792 | 1.20 g/cm³ |
| hardness | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 94 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.