plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PUR-Ester Vibrathane® 6012 CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodCHEMTURU USA/Vibrathane® 6012
Shore hardnessShoreAASTM D224094
thermal performanceTest ConditionTest MethodCHEMTURU USA/Vibrathane® 6012
Brittle temperatureASTM D746-58.0 °C
Uncured PropertiesTest ConditionTest MethodCHEMTURU USA/Vibrathane® 6012
Curing time110°C1.0 hr
thermosettingTest ConditionTest MethodCHEMTURU USA/Vibrathane® 6012
Post curing time110°C4.0 hr
Physical propertiesTest ConditionTest MethodCHEMTURU USA/Vibrathane® 6012
densityASTM D7921.20 g/cm³
elastomerTest ConditionTest MethodCHEMTURU USA/Vibrathane® 6012
elongationBreakASTM D412430 %
Permanent compression deformation70°C,22hrASTM D395B52 %
Shore hardnessASTM D263224 %
tear strengthSplitASTM D47025 kN/m
--2ASTM D624133 kN/m
tensile strengthASTM D41253.8 MPa
100%StrainASTM D41210.3 MPa