impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap23°CISO 18017 kJ/m²
Impact strength of cantilever beam gap23°CASTM D256240 J/m
flammabilityTest ConditionTest MethodTest Result
Burning wire flammability indexIEC 60695-2-12550 °C
mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldISO 527-250.0 MPa
elongationBreakASTM D63812 %
Tensile strainBreakISO 527-212 %
Bending modulusASTM D7902000 MPa
bending strengthISO 17870.0 MPa
bending strengthASTM D79070.0 MPa
Bending modulusISO 1782000 MPa
tensile strengthYieldASTM D63850.0 MPa
Tensile modulusISO 527-22400 MPa
Tensile modulusASTM D6382400 MPa
thermal performanceTest ConditionTest MethodTest Result
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A89.0 °C
Hot deformation temperature1.8MPa,UnannealedASTM D64889.0 °C
Physical propertiesTest ConditionTest MethodTest Result
densityISO 11831.04 g/cm³
melt mass-flow rate220°C/10.0kgASTM D123811 g/10min
densityASTM D7921.04 g/cm³
Shrinkage rateISO 25770.50 %
Shrinkage rateMDASTM D9550.50 %
melt mass-flow rate220°C/10.0kgISO 113311 g/10min
hardnessTest ConditionTest MethodTest Result
Rockwell hardnessR-ScaleISO 2039-2112
Rockwell hardnessR-ScaleASTM D785112
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.