Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.10 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTM D224079to85
Mechanical propertiesTest ConditionTest MethodTest Result
Wear amountDIN 5351625.0 mm³
elastomerTest ConditionTest MethodTest Result
tensile strength ASTM D4126.00 MPa
tensile strength ASTM D41210.0 MPa
tensile strength ASTM D41225.0 MPa
elongationBreakASTM D412600 %
tear strengthASTM D6240.0800 kN/m
compression setASTM D395B30 %
compression setASTM D395B40 %
Thermal performanceTest ConditionTest MethodTest Result
Glass Transition TemperatureASTM D3418-55.0 °C
melting temperature180to195 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.