Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU-Ether Utomer UT880 Shanghai Utomer Material Science Co., Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT880 |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 79to85 |
| thermal performance | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT880 |
|---|---|---|---|
| Glass transition temperature | ASTM D3418 | -55.0 °C | |
| Melting temperature | 180to195 °C |
| mechanical properties | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT880 |
|---|---|---|---|
| Wear amount | DIN 53516 | 25.0 mm³ |
| Physical properties | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT880 |
|---|---|---|---|
| density | ASTM D792 | 1.10 g/cm³ |
| elastomer | Test Condition | Test Method | Shanghai Utomer Material Science Co., Ltd./Utomer UT880 |
|---|---|---|---|
| elongation | Break | ASTM D412 | 600 % |
| Permanent compression deformation | 70°C,24hr | ASTM D395B | 40 % |
| 23°C,70hr | ASTM D395B | 30 % | |
| tear strength | ASTM D624 | 0.0800 kN/m | |
| tensile strength | ASTM D412 | 25.0 MPa | |
| 300%Strain | ASTM D412 | 10.0 MPa | |
| 100%Strain | ASTM D412 | 6.00 MPa |