Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ASTMD570 | 0.50到0.60 % |
Water absorption rate | Saturation | ASTMD570 | 2.0到2.5 % |
Water absorption rate | | ASTMD570 | 110 MPa |
density | | ASTMD792 | 1.14到1.15 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | ASTMD785 | 100到115 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 2590到3280 MPa |
tensile strength | | ASTMD638 | 65.5到75.8 MPa |
elongation | Break | ASTMD638 | 45到55 % |
Flexural modulus | | ASTMD790 | 2590到3280 MPa |
bending strength | | ASTMD790 | 96.5到110 MPa |
Compression Modulus | | ASTMD695 | 1900到2590 MPa |
compressive strength | | ASTMD695 | 82.7到96.5 MPa |
shear strength | | ASTMD732 | 55.2到62.1 MPa |
| Itself - Dynamic | ASTMD1894 | 0.12 |
Load deformation | | ASTMD621 | 0.700到0.800 % |
| | | 4.00 |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 75到96 J/m |
Tensile impact strength | | ASTMD1822 | 69.4到75.7 kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Continuous use temperature | | ASTMD794 | 110 °C |
melting temperature | | | 227到238 °C |
| | ASTMD648 | 204到221 °C |
| | ASTMD648 | 93.3到204 °C |
| | ASTMD696 | 9E-05 cm/cm/°C |
Service | | | 166 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.