Propylene Elastomer

Propylene Elastomer XP 8656ML

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD15050.916 g/cm³
melt mass-flow rateASTMD12380.50 g/10min
optical performance Test ConditionTest MethodTest Result
glossASTMD245733
Haze ratioASTMD100322 %
filmTest ConditionTest MethodTest Result
Secant modulusASTMD882186 MPa
Secant modulusASTMD882227 MPa
tensile strengthASTMD8829.00 MPa
tensile strengthASTMD8829.60 MPa
tensile strengthASTMD88272.2 MPa
tensile strengthASTMD88250.3 MPa
elongationASTMD882300 %
elongationASTMD882640 %
Falling hammer impactASTMD1709750 g
Elmondov tear strengthASTMD1922500 g
Elmondov tear strengthASTMD1922540 g
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.