Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
Propylene Elastomer XP 8656ML ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

filmTest ConditionTest MethodExxonMobil/XP 8656ML
tensile strength TD:断裂ASTM D88250.3 MPa
Elmendorf tear strengthMDASTM D1922500 g
Dart impactASTM D1709750 g
tensile strength TD:屈服ASTM D8829.60 MPa
elongationMD:断裂ASTM D882300 %
Secant modulus1%正割,TDASTM D882227 MPa
Elmendorf tear strengthTDASTM D1922540 g
tensile strength MD:断裂ASTM D88272.2 MPa
Secant modulus1%正割,MDASTM D882186 MPa
tensile strength MD:屈服ASTM D8829.00 MPa
elongationTD:断裂ASTM D882640 %
optical performance Test ConditionTest MethodExxonMobil/XP 8656ML
gloss45°ASTM D245733
Haze ratioASTM D100322 %
physical property Test ConditionTest MethodExxonMobil/XP 8656ML
densityASTM D15050.916 g/cm³
melt mass-flow rate190°C/2.16kgASTM D12380.50 g/10min

Contact Us