Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Melt volume flow rate | | | 35.0 cm3/10min |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | | ASTM D2240 | 56 |
Shore hardness | | ASTM D2240 | 15 |
Shore hardness | | DIN 53505 | 55 |
Shore hardness | | DIN 53505 | 15 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
wear resistance | | DIN 53516 | 43 mm³ |
wear resistance | | ASTM D395 | 43 mm³ |
elastomer | Test Condition | Test Method | Test Result |
---|
compression set | | ASTM D412 | 8 % |
compression set | | DIN 53504 | 8 % |
tensile strength | | ASTM D412 | 2.34 Mpa |
tensile strength | | DIN 53504 | 1.40 Mpa |
compression set | | DIN 53517 | 35 % |
compression set | | DIN 53517 | 60 % |
Shore hardness | | ASTM D2632 | 60 % |
tensile strength | | ASTM D412 | 4.07 Mpa |
tensile strength | | DIN 53504 | 2.40 Mpa |
tensile strength | | ASTM D412 | 7.52 Mpa |
tensile strength | | DIN 53504 | 10.0 Mpa |
Tensile strain | | ASTM D412 | 720 % |
Tensile strain | | DIN 53504 | 900 % |
tear strength | | ASTM D624 | 35.9 kN/m |
tear strength | | DIN 53515 | 25 kN/m |
compression set | | ASTM D395 | 40 % |
compression set | | ASTM D395 | 80 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
melting temperature | | 内部方法 | 98.9to130 °C |
TMA | | 内部方法 | 145 °C |
TMA | | 内部方法 | 110 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.