Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792 | 1.01to1.33 g/cm³ |
melt mass-flow rate | | ASTM D1238 | 5.1to16 g/10min |
Shrinkage rate | | ASTM D955 | 0.40to1.1 % |
Shrinkage rate | | ASTM D955 | 0.33to1.1 % |
Water absorption rate | | ASTM D570 | 0.059to0.23 % |
hardness | Test Condition | Test Method | Test Result |
---|
Shore hardness | | ASTM D2240 | 70to93 |
flammability | Test Condition | Test Method | Test Result |
---|
Burning wire flammability index | | IEC 60695-2-12 | 743to960 °C |
Hot filament ignition temperature | | IEC 60695-2-13 | 725to800 °C |
Limiting Oxygen Index | | ISO 4589-2 | 24to29 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
fracture | | ISO 527-2 | 8.75to23.0 MPa |
fracture | | ASTM D638 | 93to310 % |
fracture | | ISO 527-2 | 90to230 % |
fracture | | ASTM D638 | 8.50to27.4 MPa |
film | Test Condition | Test Method | Test Result |
---|
Tear resistance of pants | | ISO 6383-1 | 7.00to46.0 N/mm |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric strength | | IEC 60243-1 | 21to26 kV/mm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
UL temperature rating | | | 80to105 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.