Technical Data Sheet
processability | Test Condition | Test Method | Test Result |
---|
Melt Temperature | | | 150-170 °C |
optical performance | Test Condition | Test Method | Test Result |
---|
gloss | | ASTM D-2457 | 70 |
Haze ratio | | ASTM D-1003 | 7 % |
Basic performance | Test Condition | Test Method | Test Result |
---|
density | | ASTM D-792 | 0.923 g/m3 |
melt mass-flow rate | | ISO 1133 | 3.5 g/10min |
film thickness | | | 50 um |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tangent modulus (TD) | | ASTM D-882 | 175 Mpa |
Tangent modulus (MD) | | ASTM D-882 | 190 Mpa |
Tensile yield strength (TD) | | ASTM D-882 | 9 Mpa |
Tensile yield strength (MD) | | ASTM D-882 | 9 Mpa |
Tensile fracture strength (TD) | | ASTM D-882 | 15 Mpa |
Tensile strength at break (MD) | | ASTM D-882 | 17 Mpa |
Tensile elongation at break (TD) | | ASTM D-882 | 650 % |
Tensile elongation at break (MD) | | ASTM D-882 | 450 % |
Falling hammer impact | | ASTM D-1709A | 120 g |
Elmendorf Tear Strength (MD) | | ASTM D-1922 | 500 g |
| | ASTM D-1894 | 0.16-0.2 |
Elmendorf Tear Strength (TD) | | ASTM D-1922 | 400 g |
Thermal performance | Test Condition | Test Method | Test Result |
---|
vicat | | ISO 306/A | 93 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.