Test Condition | Test Method | Test Result | |
---|---|---|---|
Tensile strain | ASTMD882 | 870 % | |
Falling hammer impact | ASTMD1709A | 96 g | |
Elmondov tear strength MD | ASTMD1922 | 210 g | |
ElmendorfTearStrength-TD | ASTMD1922 | 220 g | |
vicat | ASTMD1525 | 63.0 °C | |
gloss | ASTMD2457 | 86 | |
Haze ratio | ASTMD1003 | 1.1 % | |
melt mass-flow rate | ASTMD1238 | 5.2 g/10min | |
Vinyl acetate content | ExxonMobilMethod | 14.9 wt% | |
Secant modulus | ASTMD882 | 77.1 MPa | |
ASTMD882 | 81.4 MPa | ||
tensile strength | Break | ASTMD882 | 29.6 MPa |
Tensile strength TD | Break | ASTMD882 | 19.4 MPa |
elongation | Break | ASTMD882 | 320 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.