Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Ethylene Copolymer Ultra LD 708.62 ExxonMobil
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Test Condition | Test Method | ExxonMobil/Ultra LD 708.62 | |
---|---|---|---|
Vinyl acetate content | ExxonMobilMethod | 14.9 wt% | |
elongation | 断裂 | ASTM D882 | 320 % |
melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 5.2 g/10min |
Dart impact | ASTM D1709A | 96 g | |
tensile strength | 断裂,TD | ASTM D882 | 19.4 MPa |
Elmendorf tear strength | MD | ASTM D1922 | 210 g |
Haze ratio | ASTM D1003 | 1.1 % | |
Tensile strain | Break | ASTM D882 | 870 % |
gloss | 45° | ASTM D2457 | 86 |
Elmendorf tear strength | TD | ASTM D1922 | 220 g |
Secant modulus | ASTM D882 | 81.4 MPa | |
tensile strength | 断裂 | ASTM D882 | 29.6 MPa |
vicat | ASTM D1525 | 63.0 °C |