Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Bound styrene | 内部方法 | 22.5to24.5 % | |
AntioxidantAdditive-VS | 内部方法 | 0.30to0.70 % | |
Oil content | ASTM D5774 | 26to29 % | |
Organic Acid | ASTM D5774 | 4.0to5.6 % | |
SolventContent-extract | 内部方法 | 29to35 % | |
Mooney viscosity | ASTM D1646 | 46to54 MU |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
sulfurization | ASTM D5289 | 1.40to3.00 dNm | |
ASTM D5289 | 3.2to6.5 min | ||
ASTM D5289 | 6.5to10.5 min | ||
ASTM D5289 | 12.0to18.5 min | ||
ASTM D5289 | 12.0to18.5 dNm |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D3185 | >9.80 MPa | |
Yield | ASTM D3185 | >18.0 MPa | |
elongation | Break | ASTM D3185 | >380 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top