Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

SBR, Unspecified SIBUR Synthetic Rubber SBR-1712 HI-AR Grade B SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | SIBUR RUSSIA/SIBUR Synthetic Rubber SBR-1712 HI-AR Grade B |
---|---|---|---|
sulfurization | MaximumTorqueMH:160°C,MDR | ASTM D5289 | 12.0to18.5 dNm |
MinimumTorqueML:160°C,MDR | ASTM D5289 | 1.40to3.00 dNm | |
Timeto50%vulcanizationT'50:160°C,MDR | ASTM D5289 | 6.5to10.5 min | |
Timeto90%vulcanizationT'90:160°C,MDR | ASTM D5289 | 12.0to18.5 min | |
Prevulcanizationstarttimets1:160°C,MDR | ASTM D5289 | 3.2to6.5 min |
physical property | Test Condition | Test Method | SIBUR RUSSIA/SIBUR Synthetic Rubber SBR-1712 HI-AR Grade B |
---|---|---|---|
AntioxidantAdditive-VS | 内部方法 | 0.30to0.70 % | |
Bound styrene | 内部方法 | 22.5to24.5 % | |
Mooney viscosity | ML1+4,100°C | ASTM D1646 | 46to54 MU |
Oil content | ASTM D5774 | 26to29 % | |
Organic Acid | ASTM D5774 | 4.0to5.6 % | |
SolventContent-extract | 内部方法 | 29to35 % |
elastomer | Test Condition | Test Method | SIBUR RUSSIA/SIBUR Synthetic Rubber SBR-1712 HI-AR Grade B |
---|---|---|---|
tensile strength | 300%应变 | ASTM D3185 | >9.80 MPa |
elongation | 断裂 | ASTM D3185 | >380 % |
tensile strength | 屈服 | ASTM D3185 | >18.0 MPa |