PBT P7408 TYNE USA

0
  • Properties:
    Glass
    mineral 40%
    performance characteristics
    improved impact resistance
    good impact resistance

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.10 g/cm3
Shrinkage rateASTM D9550.50-0.70 %
Water absorption rateASTM D5700.20 %
densityASTM D7921.10 g/cm³
Shrinkage rateASTM D9550.50to0.70 %
Water absorption rateASTM D5700.20 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D25669 J/m
Suspended wall beam without notch impact strengthASTM D256430 J/m
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength BreakASTM D63875.8 MPa
elongationYieldASTM D6382.0 %
Flexural modulusASTM D7907580 MPa
bending strengthASTM D790117 MPa
Flexural modulusASTM D7907580 MPa
bending strengthASTM D790117 MPa
Impact strength of cantilever beam gapASTM D25669 J/m
Suspended wall beam without notch impact strengthASTM D256430 J/m
Fracture tensile strengthASTM D63875.8 MPa
elongation at yieldASTM D6382.0 %
Electrical performanceTest ConditionTest MethodTest Result
Dissipation FactorASTM D1500.020
Dissipation FactorASTM D1500.020
Volume resistivityASTM D2576E+16 ohms·cm
dielectric strengthASTM D14930 kV/mm
dielectric constantASTM D1504.00
Volume resistivityASTM D2576E+16 ohm.cm
dielectric strengthASTM D14930 kV/mm
dielectric constantASTM D1504.00
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648210 °C
Heat distortion temperatureASTM D648193
Heat distortion temperatureASTM D648210
Heat distortion temperatureASTM D648193 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.