PA66 Nivionplast® A R306GY NAT
0
- Properties:Fillerglass fiber reinforced material30%filler by weight
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 1.36 g/cm³ | |
Shrinkage rate | 内部方法 | 0.40 % | |
Water absorption rate | ISO 62 | 5.5 % | |
ISO 62 | 1.9 % | ||
ash content | 内部方法 | 30 % |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
elongation | Break | ASTM D638 | 3.0 % |
Tensile modulus | ASTM D638 | 10000 MPa | |
tensile strength | Break | ASTM D638 | 180 MPa |
Flexural modulus | ASTM D790 | 8500 MPa | |
bending strength | ASTM D790 | 270 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 95 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat distortion temperature | ASTM D648 | 250 °C | |
ASTM D648 | 245 °C | ||
melting temperature | ASTM D3417 | 260 °C | |
Linear coefficient of thermal expansion | ASTM D696 | 2.5E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.