plas
Log In

TPU LARIPUR®  LARIPUR 9060 COIM ITALY

20

Technical Data Sheet

flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-2
elastomerTest ConditionTest MethodTest Result
Permanent compression deformation70°C,22hrASTM D39545 %
Permanent compression deformation23°C,70hrASTM D39525 %
tear strengthASTM D62486.0 kN/m
elongationBreakASTM D412610 %
tensile strengthBreakASTM D41246.1 Mpa
tensile strength300%StrainASTM D41212.8 Mpa
tensile strength100%StrainASTM D4126.50 Mpa
tensile strength50%StrainASTM D4124.80 Mpa
thermal performanceTest ConditionTest MethodTest Result
Vicat softening temperatureASTM D152580.0 °C
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreAASTM D224086
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.