Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU LARIPUR 9060 COIM ITALY
LARIPUR®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | COIM ITALY/LARIPUR 9060 |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 86 |
| thermal performance | Test Condition | Test Method | COIM ITALY/LARIPUR 9060 |
|---|---|---|---|
| Vicat softening temperature | ASTM D1525 | 80.0 °C |
| flammability | Test Condition | Test Method | COIM ITALY/LARIPUR 9060 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | V-2 |
| elastomer | Test Condition | Test Method | COIM ITALY/LARIPUR 9060 |
|---|---|---|---|
| elongation | Break | ASTM D412 | 610 % |
| Permanent compression deformation | 70°C,22hr | ASTM D395 | 45 % |
| 23°C,70hr | ASTM D395 | 25 % | |
| tear strength | ASTM D624 | 86.0 kN/m | |
| tensile strength | 50%Strain | ASTM D412 | 4.80 Mpa |
| Break | ASTM D412 | 46.1 Mpa | |
| 100%Strain | ASTM D412 | 6.50 Mpa | |
| 300%Strain | ASTM D412 | 12.8 Mpa |