physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.12到1.14 g/cm³ |
Water absorption rate | | ASTMD570 | 0.032 % |
hardness | Test Condition | Test Method | Test Result |
---|
Rockwell hardness | R-Scale | ASTMD785 | 113到120 |
| | ASTMD2240 | 75到84 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
| Itself - Dynamic | ASTMD1894 | 0.14到0.19 |
| Itself - Static | ASTMD1894 | 0.12到0.14 |
Tensile modulus | | ASTMD638 | 3170 MPa |
tensile strength | | ASTMD638 | 69.6到70.3 MPa |
elongation | Break | ASTMD638 | 38到47 % |
Flexural modulus | | ASTMD790 | 2510到2590 MPa |
bending strength | | ASTMD790 | 86.9到89.6 MPa |
Compression Modulus | | ASTMD695 | 1870到1970 MPa |
compressive strength | | ASTMD695 | 101到112 MPa |
shear strength | | ASTMD732 | 58.9到59.2 MPa |
Load deformation | | ASTMD621 | 0.510 % |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 74到80 J/m |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 216 °C |
| | ASTMD648 | 70.0到72.2 °C |
| Melting Temperature | ASTMD648 | 221 °C |
| | ASTMD696 | 7.5E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.