Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO1183/A | 1.11到1.15 g/cm³ | |
melt mass-flow rate | ISO1133 | 15到20 g/10min |
Impact resistance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of cantilever beam gap | ASTMD256A | 400到450 J/m | |
ASTMD256 | 无断裂 | ||
ASTMD256 | 40到45 kJ/m² | ||
ISO180/A | 35到40 kJ/m² | ||
ISO180 | 无断裂 | ||
Charpy Notched Impact Strength | ISO179/1eA | 35到40 kJ/m² | |
Impact strength of simply supported beam without notch | ISO179/1eU | 无断裂 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ISO527-2/1A/1 | 1800到2000 MPa | |
Tensile stress | Yield | ISO527-2/1A/50 | 40.0到45.0 MPa |
Break | ISO527-2/1A/50 | 40.0到45.0 MPa | |
Tensile strain | Yield | ISO527-2/1A/50 | 4.0到6.0 % |
Break | ISO527-2/1A/50 | 35到40 % | |
Flexural modulus | ISO178 | 1800到2200 MPa | |
Bending stress | ISO178 | 45.0到50.0 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD648 | 115到125 °C | ||
ISO75-2/B | 120到130 °C | ||
ASTMD648 | 100到110 °C | ||
vicat | ISO306/A120 | 125到135 °C | |
ISO306/B120 | 120到130 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.