Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| Resin | | 按重量计算的混合比:100 |
| Hardener | | 按重量计算的混合比:33 |
Thermosetting mixed viscosity | | | 3000 cP |
Thermosetting mixed viscosity | | | 18000 cP |
physical property | Test Condition | Test Method | Test Result |
---|
density | | | 1.03 g/cm³ |
density | | | 1.05 g/cm³ |
density | | | 0.33 % |
density | | | 3.6 % |
hardness | Test Condition | Test Method | Test Result |
---|
| Shore A | | 80 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|
Non volatile matter content - MixedSystem | | | 100 % |
Antifungal activity | | | Non-nutrient |
IsocyanateContent | | | 5.2 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus- | | 内部方法 | 9.65 MPa |
tensile strength | | | 34.5 MPa |
elongation | Break | | 400 % |
elastomer | Test Condition | Test Method | Test Result |
---|
compression set | | | 35 % |
tear strength | | | 35.0 kN/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|
Surface Resistivity | | | 3.5E+10 ohms |
Surface Resistivity | | | 5.2E+13 ohms |
Volume resistivity | | | 2.4E+12 ohms·cm |
Volume resistivity | | | 9.6E+10 ohms·cm |
Volume resistivity | | | 14 kV/mm |
dielectric constant | | ASTMD150 | 6.12 |
dielectric constant | | ASTMD150 | 5.06 |
dielectric constant | | ASTMD150 | >120 sec |
InsulationResistance | | | 9E+11 ohms |
InsulationResistance | | | 4.2E+09 ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.